lead crystal battery
LEAD CRYSTAL BATTERY
THE BATTERY FOR NOW AND THE FUTURE
LEAD-ACID BATTERIES
THE PROBLEM
Traditional lead-acid batteries have many defects. This is due to the inherent structural characteristics,
which include:
•
Plate sulfation
•
Active material loss
•
Dehydration
•
Serious acid pollution
•
Short cycle life
•
Poor low/high temperature characteristics
1
LEAD-ACID BATTERIES
THE SOLUTION
To overcome the structural defects in lead-acid batteries, manufacturers started using AGM and a
gel electrolyte in batteries. Although this did not solve all the problems, progress was made by:
•
•
•
•
Reducing the acid mist
Reducing the water loss rate
Reducing the self-discharge rate
Improving the discharge capacity
By solving these problems, a new series of challenges were introduced:
•
•
•
Poor electrode penetration by the gel electrolyte
Weak capacity of AGM separator match
Slow electrode reaction
2
LEAD CRYSTAL BATTERIES
THE DIFFERENCE
In order to overcome the fundamental shortcomings of the lead-acid and AGM or gel batteries, the
LEAD CRYSTAL BATTERY uses new proprietary technologies, including:
•
•
•
•
•
•
•
Silica crystalline state SiO2 composite electrolyte (NOT A GEL) to replace the conventional
sulfuric acid solution
The preparation method of the Silica crystalline state SiO2 composite electrolyte
The irrigation fluid device, and its battery plus liquid method
Battery terminals connected to protective devices
Batteries with liquid shunt valve
New plates
New AGM
3
LEAD CRYSTAL BATTERIES
DIFFERENCE RESULTS
As a result, this self-designed SiO2 cleaning composite electrolyte replaces the conventional sulfuric
acid solution/gel. A number of unique and advanced technologies are used in the manufacturing of
the Lead Crystal Battery in order to solve the lead-acid/gel battery problems. This includes:
•
•
•
•
•
•
Virtually no plate sulfation
No active material loss
No dehydration
No acid pollution
Excellent cycle life
Very good low/high temperature characteristics
4
LEAD CRYSTAL BATTERY - COMPARISON TABLE
ITEM
ACID
GEL
LED CRYSTAL
NiCad
LITHIUM
SUPERIOR
PRODUCT
Range of Working
Temperature
18°C to + 45°C
-18°C to + 50°C
-40°C to + 65°C
-20°C to + 65°C
-20°C to + 65°C
Lead Crystal
Environment
Harmful
Harmful
Friendlier
Harmful
Friendlier
Lead Crystal & Lithium
Safety Transportation
Not Good
Normal
Good
Not Good
Good
Lead Crystal & Lithium
Discharge Cycle at 80%
450
500
1000
1000
1000
Lead Crystal & Lithium
Discharge Ability at High
Current
Not Good
Not Good
Good
Good
Normal
Lead Crystal
Work Ability as a
Battery Pack
OK
OK
Good
Normal
Normal
Lead Crystal & Lithium
(Lithium needs outside
control)
Cost
Lowest
Low
Slightly Higher
than Gel
Much Higher
Highest
Acid
Battery Lifetime
Throughput Cost
per kWh
Low
High
Lowest
Highest
2nd Lowest
Lead Crystal
Battery Lifetime
Throughput kWh
5th
4th
2nd
3rd
Best
Lithium
5
THANK YOU
Was this manual useful for you? yes no
Thank you for your participation!

* Your assessment is very important for improving the work of artificial intelligence, which forms the content of this project

Download PDF

advertising